Advanced Powder Metallurgy Laboratory

Level begin

Research Facilities:

SPS from 1200 °C to 1000 °C

SPS from 800 °C to 1000 °C

SPS up to 800 °C

Magnetic Pulse Compression (MPC)

SPS (temperature above 2000 °C)

SPS (1200 °C to 1900 °C)

 

Lab description:

For SPS device

1- It is mandatory for the applicant to announce the sinter temperature, pulse specifications and pressure value

2- Calculating the amount of powder required for each sample depending on the dimensions and height desired by the applicant is his responsibility.

4- The cost of demolition of the mold, in case of combustion and explosion reactions during the test, is the responsibility of the applicant.

In case the sample causes damage to the device during the test, the applicant is responsible for compensating all damages. The maximum storage time at the desired temperature is 15 minutes.

 

-------------------------------------------------- ------------------------------------------

* University students are required to register the application and complete the form in the process management system of Isfahan University of Technology at the following address:

https://bpms.iut.ac.ir

- After confirming the request by referring to the head of the laboratory, the necessary arrangements will be made to perform the test.

-------------------------------------------------- ------------------------------------------

Tel: 03133912750 and 52

Email: m.nourbakhsh@of.iut.ac.ir

Address: Materials Engineering Department, Isfahan University of Technology,  Isfahan, 84156-83111, Iran.

 

Mohammad Nourbakhsh

Staff, Lab Instructor